How to deal with the plastic injection molding raw material is not filled?

Electric injection molding machine in the production of injection mold will encounter the situation of injection molding is not filled, there is a lack of glue at the bone position right Angle and fuse connection, here to share some experience.

Analysis of glue injection is not filled:

1. The trapped air in the bone position makes the injection molding machine fill up.

2. The filling of the injection molding machine caused by the glue welding line is not filled.

Reason analysis of glue injection is not filled:

When the injection molding machine is working, the mold gluing method is two-point gluing, and the injection speed is too fast, which is easy to cause the gas trapped at the right Angle of the bone position and cause the filling dissatisfaction; If the injection speed is too slow, it is easy to fill the fuse at the end of the flow.

The solution:

Multistage injection molding and position switching.

In the first stage, the medium speed filling channel was used to pass through the glue inlet and switch the position; then, the second stage was used to quickly fill the vicinity of the bone site and switch the position; the third stage was used to slowly fill the bone site to discharge the gas; finally, the speed filling was used to switch the pressure holding position and the pressure holding time was extended appropriately.

  • 32
    点赞
  • 13
    收藏
    觉得还不错? 一键收藏
  • 0
    评论

“相关推荐”对你有帮助么?

  • 非常没帮助
  • 没帮助
  • 一般
  • 有帮助
  • 非常有帮助
提交
评论
添加红包

请填写红包祝福语或标题

红包个数最小为10个

红包金额最低5元

当前余额3.43前往充值 >
需支付:10.00
成就一亿技术人!
领取后你会自动成为博主和红包主的粉丝 规则
hope_wisdom
发出的红包
实付
使用余额支付
点击重新获取
扫码支付
钱包余额 0

抵扣说明:

1.余额是钱包充值的虚拟货币,按照1:1的比例进行支付金额的抵扣。
2.余额无法直接购买下载,可以购买VIP、付费专栏及课程。

余额充值